Polymer Property : Specific Surface Area = 60 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 50 - 60 m²/g
50 - 60 m²/g
Zircar Zirconia ZYP-55 Zirconia Powder
Zircar Zirconia Powder Type ZYP is an ultra fine, highly reactive powder composed of yttria- stabilized zirconia. It is offered with two different surface areas; Type ZYP-55 has a surface area of 50..
Specific Surface Area 50 - 60 m²/g
50 - 60 m²/g
Zircar Zirconia ZYP-55 Zirconia Powder
Zircar Zirconia Powder Type ZYP is an ultra fine, highly reactive powder composed of yttria- stabilized zirconia. It is offered with two different surface areas; Type ZYP-55 has a surface area of 50..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Calcium Carbonate Nanoparticles
General DescriptionCalcium Carbonate (CaCO3) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Carbonate Particles are typically 10 - 80 nanometers (..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Dysprosium Nanoparticles
General DescriptionDysprosium (Dy) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Particles are typically 10 - 80 nanometers (nm) with sp..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Dysprosium Oxide Nanopowder
General DescriptionDysprosium (DyO) Oxide Nanopowder or Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Oxide Particles are typically 10 -..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Erbium Nanoparticles
General DescriptionErbium (Er) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Erbium Particles are typically 10 - 80 nanometers (nm) with specific s..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Holmium Nanoparticles
General DescriptionHolmium (Ho) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Particles are typically 30 - 80 nanometers (nm) with speci..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Niobium Nanoparticles
General DescriptionNiobium (Nb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Niobium Particles are typically 10-20 nanometers (nm) with..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Tantalum Nanoparticles
General DescriptionTantalum (Ta) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tantalum Particles are typically 10-20 nanometers (nm) wi..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Terbium Nanoparticles
General DescriptionTerbium (Tb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Terbium Particles are typically 10 - 80 nanometers (nm) with specific..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Thulium Nanoparticles
General DescriptionThulium (Tm) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Thulium Particles are typically 25 - 100 nanometers (nm) with specifi..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Tin Nanoparticles
General DescriptionTin (Sn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tin Particles are typically 10-20 nanometers (nm) with specifi..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Ytterbium Nanoparticles
General DescriptionYtterbium (Yb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Ytterbium Particles are typically 10 - 80 nanometers (nm) with spec..
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
American Elements Calcium Phosphate Nanoparticles
General DescriptionCalcium Phosphate (CAP) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Phosphate Particles are typically 10 - 80 nanometers (nm..