Material Notes:
General DescriptionDysprosium (DyO) Oxide Nanopowder or Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Oxide Particles are typically 10 - 80 nanometers (nm) with specific surface area (SSA) in the 30 – 60 m 2 /g range. Nano Dysprosium Oxide Particles are also available in passivated and Ultra high purity and high purity and coated and dispersed forms. Research into applications for Dysprosium Oxide nanocrystals has focused on use as a Magnetic Nanoparticle with numerous uses and as high surface area supports for catalytic compounds.
Physical Properties Metric English Comments
Particle Size 0.010 - 0.080 µm
0.010 - 0.080 µm
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
Molecular Weight 373 g/mol
373 g/mol
Descriptive Properties Value Comments
Appearance Black
Solubility Insoluble in water, moderately soluble in strong mineral acids
Stability Slightly hygroscopic