Material Notes:
Lucite® 41 is a high molecular weight methyl methacrylate homopolymer for use in castings & embedments.Like all Lucite® Acrylic Resins for castings & embedments, Lucite® 41 offers: Exceptional Gloss; Very High Surface Hardness and Abrasion Resistance; Sparkle; Crystal Clarity; Outstanding Ultraviolet Light Resistance; Excellent Resistance to Water, Alcohol, Dilute Acids and Alkalis, Chemical Fumes, and Corrosive and Oxidizing EnvironmentsLucite International’s Lucite® resins production process results in pure product to enable castings and embedments to be manufactured with exceptional optical clarity and sparkle.Information provided by Lucite International
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0431 lb/in³
Water Absorption 0.47 %
0.47 %
Particle Size 75 - 105 µm
75 - 105 µm
Viscosity Measurement 1.137 - 1.367
1.137 - 1.367
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Mechanical Properties Metric English Comments
Hardness, Rockwell M 81
81
Tensile Strength 55.0 MPa
7980 psi
Elongation at Break 1.0 %
1.0 %
Optical Properties Metric English Comments
Refractive Index 1.491
1.491
Transmission, Visible 92 %
92 %
Processing Properties Metric English Comments
Moisture Content 0.75 %
0.75 %