Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 64 µm | <= 64 µm | 100% |
SGL Carbon Group CF 1135 Carbon Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | <= 64 µm | <= 64 µm | 97% |
SGL Carbon Group CF 270 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | <= 64 µm | <= 64 µm | 96% |
SGL Carbon Group CF 3100 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | <= 64 µm | <= 64 µm | 82% |
SGL Carbon Group CF 480 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | <= 64 µm | <= 64 µm | 86% |
SGL Carbon Group CF 5250 Carbon Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | 64 µm | 64 µm | |
Silberline Sparkle Silvex® 755-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Particle Size | 64 µm | 64 µm | |
Silberline Sparkle Silvex® 755-20-D Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Particle Size | 64 µm | 64 µm | Before Conversion |
Silberline Sparkle Silvet® 755-30-E1 Sparkle Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final .. |