Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 60 µm | <= 60 µm | 90% smaller than |
Nyco ASPECT® 4000 Wollastonite ASPECT 4000 is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive .. |
|||
Particle Size | <= 60 µm | <= 60 µm | 90% smaller than |
Nyco M200 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | <= 60 µm | <= 60 µm | 90% smaller than |
Nyco NYAD® M200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | <= 60 µm | <= 60 µm | 90% smaller than |
Nyco NYAD® MD200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | <= 60 µm | <= 60 µm | 90% smaller than |
Nyco NYGLOS® 12 Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Particle Size | 60 - 120 µm | 60 - 120 µm | mesh. |
Oceanchem Group Xanthan Gum Oil Drilling Grade Information Provided by Oceanchem Group |
|||
Particle Size | 60 µm | 60 µm | mean value |
Potters Industries Q-Cel® 6036 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Particle Size | 60 - 70 µm | 60 - 70 µm | Mean |
Potters Industries Spheriglass® 2530 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Particle Size | 60 - 80 µm | 60 - 80 µm | |
Lucite International Colacryl ® D60 Acrylic Dental Resin A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f.. |
|||
Particle Size | 60 - 76 µm | 60 - 76 µm | |
Lucite International Colacryl ® TS2027 Acrylic Dental Resin Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.I.. |
|||
Particle Size | 60 - 70 µm | 60 - 70 µm | |
Lucite International Lucite® 4FI Glass Separation Resin Improper storage and transport of glass products (e.g. flat glass or fabricated items) can lead to costly damage caused by glass-to-glass abrasion and/or corrosion rendering it unsuitable for end-us.. |
|||
Particle Size | 60 µm | 60 µm | 95%, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 803 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 60 µm | 60 µm | Average Mean |
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-200 Hollow Spheres EXTENDOSPHERESâ„¢ XOL-200 are white aluminosilicate multicellular hollow spheres. The density of this product averages 0.25 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-200.. |
|||
Particle Size | 60 µm | 60 µm | 95%, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 603 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 60 µm | 60 µm | at a density of 2.11 g/cc |
TIMCAL TIMREX® GB98/75 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 60 µm | 60 µm | Springback 5%, pressure 0.477 t/cc |
TIMCAL TIMREX® GB98/75 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 60 µm | 60 µm | at a density of 2.11 g/cc, pressure 2.5 t/cc |
TIMCAL TIMREX® GB99/6 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 60 µm | 60 µm | Springback 5%, pressure 0.477 t/cc |
TIMCAL TIMREX® GB99/6 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 60 µm | 60 µm | D90 (Malvern) Size B |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 60 µm | 60 µm | D90 (Malvern) Size B |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 60 µm | 60 µm | TEC QSD |
Trelleborg AEM Eccospheres® SID-160Z Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Particle Size | 60 µm | 60 µm | 50th% |
3M A16/500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 60 µm | 60 µm | 50th% |
3M A20/1000 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 60 - 90 µm | 60 - 90 µm | D(0.5) |
Akzo Nobel Expancel® 091 DE 80 d30 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 60 µm | 60 µm | 50th% |
3M H20/1000 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 60 µm | 60 µm | 50th% |
3M K15 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 60 µm | 60 µm | 50th% |
3M K20 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 60 µm | 60 µm | Effective Top Size |
3M S60HS Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |