Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 50 - 80 µm | 50 - 80 µm | Median Grain Diameter |
Nabaltec GRANALOX® NM 9922 I Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 15 - 80 µm | 15 - 80 µm | |
Potters Industries Sphericel® 25P45 Hollow Engineered Glass Microspheres Sphericel® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strength.. |
|||
Particle Size | 40 - 80 µm | 40 - 80 µm | d50 |
Magyar Aluminum ALOLT 01 Aluminum Hydroxide Dry type |
|||
Particle Size | 60 - 80 µm | 60 - 80 µm | |
Lucite International Colacryl ® D60 Acrylic Dental Resin A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f.. |
|||
Particle Size | 20 - 80 µm | 20 - 80 µm | |
DayGlo Gem-Tone GC-13P Ruby Red Gem-Tone® GC-13P Ruby Red is a rich, strong blue shade red colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use.. |
|||
Particle Size | 20 - 80 µm | 20 - 80 µm | |
DayGlo Gem-Tone GC-18F Emerald Green Gem-Tone® GC-18F Emerald Green is a rich, strong green colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use of .. |
|||
Particle Size | 20 - 80 µm | 20 - 80 µm | |
DayGlo Gem-Tone GC-19F Sapphire Blue Gem-Tone™ Sapphire Blue is a rich blue colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use of this colorant. N.. |
|||
Particle Size | 1.0 - 80 µm | 1.0 - 80 µm | 95% in range |
Arkema Group PLATAMID® H106 PA80 Powder Copolyamide Platamid® H106 PA powder is a special purpose, medium melting point, very low viscosity, thermoplastic copolyamide adhesive suitable for thermal bonding and laminating of textile and foam substrate.. |
|||
Particle Size | 50 - 80 µm | 50 - 80 µm | D(0.5) |
Akzo Nobel Expancel® 551 DE 80 d42 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 50 - 80 µm | 50 - 80 µm | D(0.5) |
Akzo Nobel Expancel® 551 WE 80 d36 Wet expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |