Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Particle Size = 90 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 5.0 - 90 µm
5.0 - 90 µm
range
Potters Industries Q-Cel® 6042S
Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat..
Particle Size 45 - 90 µm
45 - 90 µm
Range
Potters Industries Spheriglass® 2530 Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..
Particle Size 70 - 90 µm
70 - 90 µm
Laser Light Scattering Method; LSY-QB-ID016
LG Chemical Lutex 760 SBR Latex
Description: Binding Force, Print gloss, High Shear Rheology, Post Treatment Properties, Coater RunnabilityApplication: Art Paper, Paperboard-Single, Top-Film, Blade Coater, Adhesive coated paper an..
Particle Size 50 - 90 µm
50 - 90 µm
Diameter average; AN2013
Solvay JAGUAR® C 162 Surfactant
Description: Clear grade with light hair feel. Enhanced deposition of dimethicone oil on damaged hair.Chemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name: HYDROXYPROPYL GUAR HYDROXYPROPYLTRIMON..
Particle Size 60 - 90 µm
60 - 90 µm
D(0.5)
Akzo Nobel Expancel® 091 DE 80 d30 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Copyright © lookpolymers.com All Rights Reserved