Polymer Property : Particle Size = 106 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 53 - 106 µm
53 - 106 µm
Range
Potters Industries Spheriglass® 2429 Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..
Particle Size 74 - 106 µm
74 - 106 µm
Lucite International Colacryl ® TS 1649 Acrylic Orthodontic Polymer
A range of methacrylate based copolymers designed for the manufacture of high quality orthodontic dental resins.Features: Excellent dry flow characteristics; Closely controlled particle size; Contai..
Particle Size 5.0 - 106 µm
5.0 - 106 µm
Trelleborg Fillite® 106 Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..