Lucite International Colacryl ® TS 1649 Acrylic Orthodontic Polymer

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Colacryl ®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Colacryl ® TS 1649 Acrylic Orthodontic Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A range of methacrylate based copolymers designed for the manufacture of high quality orthodontic dental resins.Features: Excellent dry flow characteristics; Closely controlled particle size; Contains residual peroxide initiator; Auto-polymerises with recommended liquid; Even monomer absorption; Accurate powder flow control; Excellent slump resistance; Good build control; Good clarityInformation provided by Lucite International
Physical Properties Metric English Comments
Particle Size 74 - 106 µm
74 - 106 µm
Molecular Weight 900000 - 1.50e+6 g/mol
900000 - 1.50e+6 g/mol
Processing Properties Metric English Comments
Cure Time 20.0 min

@Pressure 0.207 MPa,
Temperature 40.0 °C
0.333 hour

@Pressure 30.0 psi,
Temperature 104 °F
Descriptive Properties Value Comments
Residual peroxide (%) .39 - .61