Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.80 - 1.1 µm | 0.80 - 1.1 µm | d10 |
Indium Corp. In(OH)3 Fine Indium Hydroxide Indium Acetate is a white powder. Fine Powder Form: Primary particles range from 0.1 to 1.0 microns in size. they range in shape from spherical to elliptical to cylindrical. Agglomerates can be .. |
|||
Particle Size | 0.70 - 1.1 µm | 0.70 - 1.1 µm | d10 |
Indium Corp. In2O3 Type B Indium Oxide, Fine Powder Indium Sesquioxide is a yellow colored powder. It is a stable ceramic-like material, insoluble in water and volatizes at 850°C. Indium sesquioxide is a n-type semiconductor and as such is used .. |