Material Notes:
Indium Acetate is a white powder. Fine Powder Form: Primary particles range from 0.1 to 1.0 microns in size. they range in shape from spherical to elliptical to cylindrical. Agglomerates can be up to 5 microns.PropertiesChemical Formula: In(OH)3Purity Grade Available: 4N (99.99%), 5N (99.999%)Solubility: Soluble in mineral acids; insoluble in water.UsesChemical synthesis.Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Particle Size 0.80 - 1.1 µm
0.80 - 1.1 µm
d10
1.4 - 2.5 µm
1.4 - 2.5 µm
d50
1.1 - 7.2 µm
1.1 - 7.2 µm
d90
Specific Surface Area 50 - 65 m²/g
50 - 65 m²/g
BET
Molecular Weight 165.84 g/mol
165.84 g/mol
Component Elements Properties Metric English Comments
Indium, In 63.9 - 67.3 %
63.9 - 67.3 %
69.24 %
69.24 %
Theoretical