Polymer Property : Particle Size = 0.700 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 0.700 µm
0.700 µm
Average Stokes Equivalent Diameter
KaMin Polyfil® WC-426 Kaolin Clay - Calcined
Fine particle size vinyl-functional calcined clay for outstanding wet electricals and long term stability in wire and cable applications.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rub..