KaMin Polyfil® WC-426 Kaolin Clay - Calcined

Category Ceramic , Clay , Kaolin Clay
Manufacturer KaMin LLC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KaMin Polyfil® WC-426 Kaolin Clay - Calcined.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fine particle size vinyl-functional calcined clay for outstanding wet electricals and long term stability in wire and cable applications.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, EPDM, Wire & CableInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Brightness 93 %
93 %
Reflectance (TAPPI)
Oil Absorption 65 %
65 %
Moisture Absorption at Equilibrium <= 0.5 %
<= 0.5 %
As Produced
Particle Size 0.700 µm
0.700 µm
Average Stokes Equivalent Diameter
1.50 µm
1.50 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.01% Retained
pH 6
6
100 g/250 ml H2O Slurry
Specific Surface Area 15.0 m²/g
15.0 m²/g
BET
Descriptive Properties Value Comments
CAS Number Proprietary
Crystalline Silica (quartz) <0.1%
Physical Form Dry
Shipping Point Macon, GA