Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.700 µm | 0.700 µm | Average Stokes Equivalent Diameter |
KaMin Polyfil® WC-426 Kaolin Clay - Calcined Fine particle size vinyl-functional calcined clay for outstanding wet electricals and long term stability in wire and cable applications.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rub.. |