Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.63 - 1.93 g/cc | 0.0589 - 0.0697 lb/in³ | Green |
CeramTec Ceramtape GC Glass Ceramic LTCC (Low Temperature Cofired Ceramic) is a new type of ceramic film developed by CeramTec AG's Electronics division. With the aid of these ceramics and their almost shrinkage-free sintering process.. |