Polymer Property : Bulk Density = 0.0697 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.63 - 1.93 g/cc
0.0589 - 0.0697 lb/in³
Green
CeramTec Ceramtape GC Glass Ceramic
LTCC (Low Temperature Cofired Ceramic) is a new type of ceramic film developed by CeramTec AG's Electronics division. With the aid of these ceramics and their almost shrinkage-free sintering process..