Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.440 g/cc | 0.0159 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons CORAX® N 660 ASTM Carbon Black Standard grade of furnace black in accordance with the requirements of ASTM D 1765Soft Black - carcass grade, semi-reinforcing carbon blackInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.440 g/cc | 0.0159 lb/in³ | ASTM D4894 |
3M Dyneon™ CC191-HE Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of high elongation 23% carbon / 2% graphite blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Bulk Density | >= 0.440 g/cc | >= 0.0159 lb/in³ | Unpacked Bulk Density |
Zoltek Panex 35® Milled Carbon Fibers Milled Carbon FibersApplications include: Buoyancy, RFI/EMI Shielding, Static Dissipation, Surface Reinforcement, Low Cost Polyurethane Friction Compounds |
|||
Bulk Density | 0.440 g/cc | 0.0159 lb/in³ | |
DuPont™ Nomex® 419 Paper, 13 mil Nominal Thickness Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: .. |
|||
Bulk Density | 0.440 g/cc | 0.0159 lb/in³ | tap; ASTM D4164 |
3D Systems DuraForm® Flex Thermoplastic Elastomer for SLS® Systems Thermoplastic elastomer material with rubber-like flexibility and functionality. For use with all selective laser sintering SLS® systems.ApplicationsAthletic footwear and equipmentGaskets, hoses an.. |
|||
Bulk Density | 0.440 g/cc | 0.0159 lb/in³ | ASTM D1895 |
ALM PA 601-CF Filled Nylon 12 Prototyping Polymer Carbon fiber filled nylon 12 easy to process, strong light weight filled material.Low density, good dimensional stability while maintaining excellent mechanical properties.Fibers have been optimized.. |
|||
Bulk Density | 0.440 g/cc | 0.0159 lb/in³ | |
Asahi Glass Fluon® G190 PTFE Granular Powder Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc. |