Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons CORAX® N 330 ASTM Carbon Black Standard grade of furnace black in accordance with the requirements of ASTM D 1765Hard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons ECORAX® 1990 Carbon Black Specialty black for tire treads and bodies that provide reduced rolling resistanceInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | |
Zircar Zirconia YF-100 Yttria Felt Insulation Yttria (yttrium oxide - Y2O3) is typically used as a stabilizer for zirconia. It is offered here in its pure and stable metal oxide form, which is not attacked by most molten metals, including lithi.. |
|||
Bulk Density | 0.370 - 0.430 g/cc | 0.0134 - 0.0155 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 90 L Refractory Insulating Castable Description: Golite 90 L is a castable with an extremely low density, used at places where a very good insulation is required.Remarks: These values apply to cast products. Also available in gunning .. |
|||
Bulk Density | >= 0.370 g/cc | >= 0.0134 lb/in³ | LSY-QB-KD019 |
LG Chemical PA828 Processing aid Description: High molecular weightApplication: Foam, soft product etcInformation provided by LG Chemical |
|||
Bulk Density | >= 0.370 g/cc | >= 0.0134 lb/in³ | LSY-QB-KD019 |
LG Chemical PA930 Processing aid Description: Ultra high molecular weightApplication: Foam, soft product etcInformation provided by LG Chemical |
|||
Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | |
Zircar Zirconia YF-100 Yttria Felt Insulation Yttria (yttrium oxide - Y2O3) is typically used as a stabilizer for zirconia. It is offered here in its pure and stable metal oxide form, which is not attacked by most molten metals, including lithi.. |
|||
Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | |
Daikin POLYFLON L-2 PTFE Low Polymer, White Fine Powder White fine powder.Major Uses: Suited especially to applications requiring fine dispersion of particles. Mold lubrication/separation compounding agent for dry lubricants, paints, plastics, rubber, p.. |
|||
Bulk Density | 0.370 - 0.450 g/cc | 0.0134 - 0.0163 lb/in³ | |
Akzo Nobel Expancel® 930 MB 120 Masterbatch with unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | |
Asahi Glass Fluon® L169J PTFE Lubricant Fluon®PTFE lubricants are used as additive to plastics, rubbers, paints, greases and so on. Frictional resistance decreases and non-stick increases on the applied surface.Information provided by As.. |
|||
Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | ASTM D1895 |
ALM PA-640-GSL Filled Nylon 12 Prototyping Polymer This carbon fiber/glass sphere filled composite is an easy to process, extremely light weight filled PA 12 material.Improved dimensional stability, recyclability, and increased stiffness.Good Z dire.. |
|||
Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | ASTM D1895 |
ALM TPE-210-S Prototyping Polymer A thermoplastic elastomer used to produce parts with “rubber like” qualities. TPE 210-S exhibits good feature definition and infiltration with polyurethane will impart even higher toughness and ab.. |
|||
Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | ASTM D4894-98a |
3M Dyneon™ TF 1750 PTFE Meets ASTM D4894 Type IINon-free-flowing powder gradeVery fine particle sizeGood electrical and mechanical propertiesLow molding pressureUsed in large billet moldingExcellent for production of very .. |