Polymer Property : Bulk Density = 0.0155 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.370 - 0.430 g/cc
0.0134 - 0.0155 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 90 L Refractory Insulating Castable
Description: Golite 90 L is a castable with an extremely low density, used at places where a very good insulation is required.Remarks: These values apply to cast products. Also available in gunning ..