Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.350 - 0.450 g/cc | 0.0126 - 0.0163 lb/in³ | |
Pau Tai UNINOX AM-929 Acrylic Impact Modifier UNINOX AM-929 is acrylic impact modified resin. It is the most efficient high impact modifier for rigid PVC and other polymers, and recommended for use in calendered sheets, extruded pipe, foam prof.. |
|||
Bulk Density | 0.250 - 0.450 g/cc | 0.00903 - 0.0163 lb/in³ | |
Magyar Aluminum ALOLT 90DLS Aluminum Hydroxide Fine Precipitated Type |
|||
Bulk Density | 0.200 - 0.450 g/cc | 0.00723 - 0.0163 lb/in³ | |
Magyar Aluminum ALOLT 90F Aluminum Hydroxide Fine Precipitated Type |
|||
Bulk Density | 0.350 - 0.450 g/cc | 0.0126 - 0.0163 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ HA Hollow Spheres EXTENDOSPHERESâ„¢ HA are off white, low-cost, low-density, high alumina, ceramic hollow spheres.Applications: Hollow spheres are ideal for use in coatings, sealants, caulks and other applications.. |
|||
Bulk Density | 0.300 - 0.450 g/cc | 0.0108 - 0.0163 lb/in³ | |
Shandong Dongyue Polymer DF-11 PTFE Molding Powder (Micronized Particles) Usage: The resin is mainly used as an insulating film for electric applications, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, and loop.Packing: PTFE is packed in .. |
|||
Bulk Density | 0.300 - 0.450 g/cc | 0.0108 - 0.0163 lb/in³ | |
Shandong Dongyue Polymer DF-16 PTFE Molding Powder (Micronized Particles) Usage: The resin can be used as the general required electric source, which is suitable for making film, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, loop, fillin.. |
|||
Bulk Density | 0.300 - 0.450 g/cc | 0.0108 - 0.0163 lb/in³ | |
Shandong Dongyue Polymer DF-17 PTFE Molding Powder (Micronized Particles) Usage: The resin is mainly used as the packing products resource and packing pelletized resource, which can be processed to film, the products of thin wall, seal, gasket, club, panel, tube, axletree.. |
|||
Bulk Density | 0.350 - 0.450 g/cc | 0.0126 - 0.0163 lb/in³ | |
Trelleborg Fillite® 160 Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.350 - 0.450 g/cc | 0.0126 - 0.0163 lb/in³ | |
Trelleborg Fillite® 52/7S (355) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.350 - 0.450 g/cc | 0.0126 - 0.0163 lb/in³ | |
Trelleborg Fillite® FG (300) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.350 - 0.450 g/cc | 0.0126 - 0.0163 lb/in³ | |
Trelleborg Fillite® 106 Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.350 - 0.450 g/cc | 0.0126 - 0.0163 lb/in³ | |
Trelleborg Fillite® SG (500) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.370 - 0.450 g/cc | 0.0134 - 0.0163 lb/in³ | |
Akzo Nobel Expancel® 930 MB 120 Masterbatch with unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Bulk Density | 0.350 - 0.450 g/cc | 0.0126 - 0.0163 lb/in³ | |
Trelleborg Fillite® PG (300LF) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |