Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.256 g/cc | 0.00926 lb/in³ | Loose |
CIMBAR CIMTUFF® 9103 Talc CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® .. |
|||
Bulk Density | 0.256 g/cc | 0.00926 lb/in³ | Loose |
CIMBAR CIMTUFF® 9103s Talc CIMTUFF® 9103s talc is a treated talc produced from high purity ore, which provides low iron content, low surface area and superior color in dry form as well as when incorporated with resins. CIMT.. |
|||
Bulk Density | 0.256 g/cc | 0.00926 lb/in³ | Loose |
CIMBAR MV 603 Talc MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are pla.. |