Polymer Property : Bulk Density = 0.00926 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.256 g/cc
0.00926 lb/in³
Loose
CIMBAR CIMTUFF® 9103 Talc
CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® ..
Bulk Density 0.256 g/cc
0.00926 lb/in³
Loose
CIMBAR CIMTUFF® 9103s Talc
CIMTUFF® 9103s talc is a treated talc produced from high purity ore, which provides low iron content, low surface area and superior color in dry form as well as when incorporated with resins. CIMT..
Bulk Density 0.256 g/cc
0.00926 lb/in³
Loose
CIMBAR MV 603 Talc
MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are pla..