Physical Properties Metric English Comments
Bulk Density 2.07 g/cc
0.0747 lb/in³
As Placed
Stellar Canada CERAMITE® SFR Wear Resistant Castable
Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w..
Bulk Density 2.07 g/cc
0.0747 lb/in³
As received
BNZ Materials No. 2986 Mortar
No. 2986 is a highly refractory mortar very similar to Blakbond, but gray to tan in color. Temperature to 3000°F.Information provided by BNZ Materials Inc.