BNZ Materials No. 2986 Mortar

Category Ceramic , Oxide , Silicon Oxide
Manufacturer BNZ Materials, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BNZ Materials No. 2986 Mortar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
No. 2986 is a highly refractory mortar very similar to Blakbond, but gray to tan in color. Temperature to 3000°F.Information provided by BNZ Materials Inc.
Physical Properties Metric English Comments
Bulk Density 2.02 g/cc
0.0729 lb/in³
Dipping, 4% H2O
2.07 g/cc
0.0747 lb/in³
As received
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00362 GPa
0.525 ksi
Dipped Joint; ASTM C198
0.0276 GPa
4.00 ksi
Mortar
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1650 °C
3000 °F
Shrinkage 5.0 %
5.0 %
Permanent Linear Change at Use Limit
Component Elements Properties Metric English Comments
Al2O3 46.3 %
46.3 %
CaO 0.20 %
0.20 %
Fe2O3 1.5 %
1.5 %
K2O 0.90 %
0.90 %
Loss on Ignition(%) 1.2 %
1.2 %
Na2O 2.4 %
2.4 %
SiO2 46.8 %
46.8 %
TiO2 1.1 %
1.1 %