Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.30 g/cc | 0.0470 lb/in³ | Apparent Density of Granules |
NYC YT3WBQ Y2O3 CIP (Cold Isostatic Pressing) Granules 99.9% and better high purity granules produce high quality finished ceramics. Uses include semiconductors / LCD industries, metallurgy, magnets, and electroceramics.Acrylic binder systemExcellent g.. |
|||
Bulk Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
Victrex® PEEK 150PF Easy Flow Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, easy flow, FDA food contact compliant, .. |
|||
Bulk Density | <= 1.30 g/cc | <= 0.0470 lb/in³ | |
Magyar Aluminum ALOLT 1AF Aluminum Hydroxide Dry type |
|||
Bulk Density | 1.30 g/cc | 0.0470 lb/in³ | of Dry Beads |
Mo-Sci Corporation GL-0191 Soda-Lime Glass Spheres Appearance: Solid soda-lime glass beads with light green color in powder formTypical applications of GL0191 beads include: spacer material for gauge control, coating, filler for plastic, retroreflec.. |
|||
Bulk Density | 1.30 g/cc | 0.0470 lb/in³ | of Dry Beads |
Mo-Sci Corporation GL-0191-S Soda-Lime Glass Spheres Appearance: Solid soda-lime glass microspheres that appear colorlessTypical applications of GL0191S glass microspheres include: grinding, mixing media, filter aids, filter media, and thermal expansi.. |
|||
Bulk Density | 1.30 g/cc | 0.0470 lb/in³ | of Dry Beads |
Mo-Sci Corporation GL-0252 Blue Soda-Lime Glass Spheres Appearance: Solid soda-lime glass microspheres with light blue color in powder form.Typical applications of GL-0252 glass microspheres include: spacer for gauge control, thermal expansion reduction .. |
|||
Bulk Density | 1.30 g/cc | 0.0470 lb/in³ | of Dry Beads |
Mo-Sci Corporation GL-0262 Ni Coated Soda-Lime Glass Spheres Appearance: Solid soda-lime glass microspheres with metallic nickel coatingTypical applications of GL-0262 glass microspheres include: conductive filler for plastic, pigment, and etc.Information pro.. |
|||
Bulk Density | 1.30 g/cc | 0.0470 lb/in³ | of Dry Beads |
Mo-Sci Corporation GL-0275-S Class VI Soda-Lime Spheres Appearance: Solid soda-lime glass microspheres with light green color in powder form.Typical applications of GL0275-S beads including: high temperature spacer material for gauge control, coating, fi.. |
|||
Bulk Density | 1.30 g/cc | 0.0470 lb/in³ | of Dry Beads |
Mo-Sci Corporation GL-0279 Silver Coated Soda-Lime Glass Spheres Appearance: Solid soda-lime glass microspheres with metallic silver coating.Typical applications of GL0279 beads including: conductive filler for plastic, pigment, and etc.Information provided by Mo.. |
|||
Bulk Density | 1.30 - 1.70 g/cc | 0.0470 - 0.0614 lb/in³ | apparent |
Indium Corp. Germanium Corporation® GeO2 Germanium Dioxide Germanium dioxide is a white powder that is manufactured in both crystalline and amorphous forms. Germanium dioxide's refractive index (1.7) and its optical dispersion properties are useful for mak.. |
|||
Bulk Density | 1.30 g/cc | 0.0470 lb/in³ | of Dry Beads |
Mo-Sci Corporation GL-0271 E-Glass Spheres Appearance: Solid low alkali E-glass beads with greenish color.Chemical Durability: Weight loss @ 90°C for 24 hrs in 5% HCl 0.3 mg/cm2Information provided by Mo-Sci Corporation. |
|||
Bulk Density | 1.30 - 1.75 g/cc | 0.0470 - 0.0632 lb/in³ | |
Sinotek Materials CFC Carbon Heat Insulation Material Information provided by Sinotek |
|||
Bulk Density | 1.30 g/cc | 0.0470 lb/in³ | |
Sharadaa Ceramics HICCS Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 1.30 g/cc | 0.0470 lb/in³ | |
Chosun Refractories LWB-135 Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 1.30 - 1.40 g/cc | 0.0470 - 0.0506 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE MW Refractory Insulating Castable Description: Golite MW (medium weight) is composed of a light weight refractory aggregate plus several additives to improve the mechanical properties.Remarks: These values apply to cast products. Al.. |