Material Notes:
Germanium dioxide is a white powder that is manufactured in both crystalline and amorphous forms. Germanium dioxide's refractive index (1.7) and its optical dispersion properties are useful for making wide-angle lenses and optical microscope objective lenses. It is transparent to infrared light.Germanium dioxide is also used as a catalyst in the production of polyethylene terephthalate (PET) resin and in the production of other germanium compounds, as well as some phosphors and semiconductor materials.Characteristics:Synonyms: Germanium (IV) Oxide, GeO2CAS Number: 1310-53-8EC Number: 215-180-8RTECS: LY5240000Purity: 99.999%Appearance/Form: White powderCrystal structure: HexagonalSolubility: Soluble in Alkalis. Slightly Soluble in Acids. Slightly soluble in Water.Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Bulk Density 1.30 - 1.70 g/cc
0.0470 - 0.0614 lb/in³
apparent
Loss On Ignition <= 3.0 %
<= 3.0 %
Molecular Weight 104.61 g/mol
104.61 g/mol
Maximum Moisture Content <= 1.0
<= 1.0
Typical, LOD
<= 2.0
<= 2.0
LOD
Thermal Properties Metric English Comments
Melting Point 1115 °C
2039 °F
Optical Properties Metric English Comments
Refractive Index 1.70
1.70
IR Transmittance 90 %
90 %
transparent; thickness not quantified
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00030 %
<= 0.00030 %
Max
Cobalt, Co <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00030 %
<= 0.00030 %
Max
Copper, Cu <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00030 %
<= 0.00030 %
Max
Germanium, Ge 69.434 %
69.434 %
Theoretical
Iron, Fe <= 0.00020 %
<= 0.00020 %
Typical
<= 0.00030 %
<= 0.00030 %
Max
Nickel, Ni <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00030 %
<= 0.00030 %
Max
Trace Metals <= 0.00030 %
<= 0.00030 %
Total combined metals, typical
<= 0.0010 %
<= 0.0010 %
Total combined metals, max
Zinc, Zn <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00030 %
<= 0.00030 %
Max
Chemical Properties Metric English Comments
Ionic Impurities - Cl (Chloride) <= 500 ppm
<= 500 ppm
Copyright © lookpolymers.com All Rights Reserved