Polymer Property : Bulk Density = 0.0275 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.700 - 0.760 g/cc
0.0253 - 0.0275 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 95 Refractory Insulating Castable
Description: Golite 95 is widely applied as an insulating backlining behind a dense castable, especially in the petrochemical industry.Remarks: These values apply to cast products. Also available in..