Polymer Property : Bulk Density = 0.0255 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.705 g/cc
0.0255 lb/in³
loose
Imerys Minsparâ„¢ 200 Feldspar
Minspar 200 is 200 mesh flotation grade soda Feldspar used in the ceramic whiteware industry for sanitaryware, dinnerware, floor and wall tile, artware and glazes.Information provided by Imerys
Bulk Density 0.705 - 0.769 g/cc
0.0255 - 0.0278 lb/in³
Aggregate, dried, 4 x 6 mesh
St. Cloud Natural Zeolite (Clinoptilolite)
Natural zeolites are microporous volcanic minerals with sieving and cation exchange properties for use in agriculture, environmental and industrial applications. Features such as a vary large inter..
Bulk Density 0.705 g/cc
0.0255 lb/in³
As Supplied
Skamol Group SKAMOCAST 14-105 Insulating Castable
SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f..