Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 18.5 cm @Thickness 1.00 mm |
7.28 in @Thickness 0.0394 in |
370°C nozzle, 180°C tool |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
Spiral Flow | 18.5 cm @Thickness 1.00 mm |
7.28 in @Thickness 0.0394 in |
370°C nozzle, 180°C tool |