Polymer Property : Spiral Flow = 16.1 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 41.0 cm

@Thickness 3.00 mm
16.1 in

@Thickness 0.118 in
385°C nozzle, 190°C tool
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
Spiral Flow 41.0 cm

@Thickness 3.00 mm
16.1 in

@Thickness 0.118 in
385°C nozzle, 190°C tool; Victrex
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
Spiral Flow 41.0 cm

@Thickness 3.00 mm
16.1 in

@Thickness 0.118 in
415°C nozzle, 210°C tool
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced