Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 2.0 - 4.5 cSt | 2.0 - 4.5 cSt | |
Unipetrol Grade B Diesel Oil Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap.. |
|||
Viscosity Measure | 2.0 - 4.5 cSt | 2.0 - 4.5 cSt | |
Unipetrol Grade D Diesel Oil Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap.. |
|||
Viscosity Measure | 2.0 - 4.5 cSt | 2.0 - 4.5 cSt | |
Unipetrol Grade F Diesel Oil Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap.. |