Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 100 - 6000 cSt | 100 - 6000 cSt | Kinetic/Kinematic |
Dow Corning 5225C Formulation Aid A 10% dispersion of high molecular weight silicone polyether in cyclopentasiloxane fluid for use in skincare, suncare, hair care, color cosmetic, and antiperspirant / deodorant applications. INCI Na.. |