Polymer Property : Linear Mold Shrinkage, Transverse = 0.040 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific)
LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific)
LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific)
LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly
LNP* THERMOCOMP* KZ001L is a compound based on Acetal Copolymer resin containing 5% Milled Glass. Added features of this material include: Low Extractible.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KZ001L is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Low Extractible.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon FX97333 PE
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon FX97333 PE
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific)
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific)
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific)
LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific)
LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66
LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.