Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0095 cm/cm @Time 86400 sec |
0.0095 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Linear Mold Shrinkage, Transverse | 0.0095 cm/cm @Time 86400 sec |
0.0095 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP MF004AS PP LNP THERMOCOMP* MF004AS is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0095 cm/cm @Time 86400 sec |
0.0095 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOTUF WF003I Polyester, TP LNP THERMOTUF* WF003I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact. |