Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 50.0 - 65.0 g/m² | 31.3 - 40.6 lb/ream | per side |
ArcelorMittal Extragal® Z100 Double-sided pure zinc galvanized steel Applications: Because of their high corrosion protection capacity and surface quality, Extragal® coated products are recommended for numerous automotive applications, for both visible and non-visib.. |
|||
Coating Weight | 50.0 - 65.0 g/m² | 31.3 - 40.6 lb/ream | per side |
ArcelorMittal Ultragal® Z100 Zinc coatings and thin organic coating Applications: With its ability to limit repeated waviness during deformation, combined with the proven qualities of Extragal(surface quality, corrosion protection), Ultragal is a coating specificall.. |
|||
Coating Weight | 40.0 - 65.0 g/m² | 25.0 - 40.6 lb/ream | |
ArcelorMittal ZF100 Galvannealed zinc-iron alloy coated steel Applications: The excellent corrosion protection and high surface quality offered by Galvannealed coatings make these products well suited for numerous automotive applications involving both visible.. |