Coating Weight 50.0 - 65.0 g/m²
31.3 - 40.6 lb/ream
per side
ArcelorMittal Extragal® Z100 Double-sided pure zinc galvanized steel
Applications: Because of their high corrosion protection capacity and surface quality, Extragal® coated products are recommended for numerous automotive applications, for both visible and non-visib..
Coating Weight 50.0 - 65.0 g/m²
31.3 - 40.6 lb/ream
per side
ArcelorMittal Ultragal® Z100 Zinc coatings and thin organic coating
Applications: With its ability to limit repeated waviness during deformation, combined with the proven qualities of Extragal(surface quality, corrosion protection), Ultragal is a coating specificall..
Coating Weight 40.0 - 65.0 g/m²
25.0 - 40.6 lb/ream
ArcelorMittal ZF100 Galvannealed zinc-iron alloy coated steel
Applications: The excellent corrosion protection and high surface quality offered by Galvannealed coatings make these products well suited for numerous automotive applications involving both visible..