Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 40.0 - 65.0 g/m² | 25.0 - 40.6 lb/ream | |
ArcelorMittal ZF100 Galvannealed zinc-iron alloy coated steel Applications: The excellent corrosion protection and high surface quality offered by Galvannealed coatings make these products well suited for numerous automotive applications involving both visible.. |