Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 35.5 g/m² | 22.2 lb/ream | ExxonMobil Method |
ExxonMobil Bicor® 150 ASB-X OPP Film Product Description: Bicor ASB-X is a two side coated, sealable OPP film designed for broad use in many applications, including overwrap, horizontal, and vertical packaging. This film is suitable as.. |
|||
Coating Weight | 35.5 g/m² | 22.2 lb/ream | 0.5 m<sup>2</sup>; ASTM E252 |
DuPont Teijin Films Mylar® RL31 Polyester Film, 100 Gauge Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Myl.. |