Coating Weight 35.5 g/m²
22.2 lb/ream
ExxonMobil Method
ExxonMobil Bicor® 150 ASB-X OPP Film
Product Description: Bicor ASB-X is a two side coated, sealable OPP film designed for broad use in many applications, including overwrap, horizontal, and vertical packaging. This film is suitable as..
Coating Weight 35.5 g/m²
22.2 lb/ream
0.5 m<sup>2</sup>; ASTM E252
DuPont Teijin Films Mylar® RL31 Polyester Film, 100 Gauge
Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Myl..