Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Bicor® 150 ASB-X OPP Film

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Bicor®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Bicor® 150 ASB-X OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Bicor ASB-X is a two side coated, sealable OPP film designed for broad use in many applications, including overwrap, horizontal, and vertical packaging. This film is suitable as an unsupported web or in a lamination. It can be surface printed, reverse printed or used unprinted.Availability: Latin America, North America and South AmericaKey Features:Outstanding optical propertiesRobust machinabilityLow and consistent COFExcellent flavor and aroma barrierExcellent heat seal strength and hot tackVery good moisture barrierGood Oxygen barrierFeatures:Acrylic CoatedFlavor & Aroma BarrierGas BarrierIn Lamination Lap SealableMoisture BarrierOxygen BarrierPVdC CoatedSealable PVdC CoatedApplications:Biscuits/Cookie/CrackersBox OverwrapConfectionery, SugarUses:Box Overwrap Flexible PackagingHFFS Flexible PackagingPre-made Bags - Flexible PackagingVFFS Flexible PackagingProcessing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Water Vapor Transmission 3.60 g/m²/day
0.232 g/100 in²/day
38°C, 90% RH
Oxygen Transmission Rate 70.0 cc/m²/day
4.51 cc/100 in²/day
23°C, 0% RH; ExxonMobil Method
Thickness 38.1 microns
1.50 mil
Nominal; ExxonMobil Method
Coating Weight 35.5 g/m²
22.2 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Coefficient of Friction 0.23
0.23
ExxonMobil Method
Film Tensile Strength at Break, MD 124 MPa
18000 psi
ExxonMobil Method
Film Tensile Strength at Break, TD 234 MPa
34000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD -4.5 %
-4.5 %
at 275°F; ExxonMobil Method
Shrinkage, TD -3.0 %
-3.0 %
at 275°F; ExxonMobil Method
Optical Properties Metric English Comments
Haze 1.2 %
1.2 %
ExxonMobil Method
Gloss 98 %
98 %
45º; ExxonMobil Method
Descriptive Properties Value Comments
Crimp Seal MST 190°F
PVdC/PVdC, 200g/in
Crimp Seal Strength 750 g/in
PVdC/PVdC, 260°F, 20psi, 3/4sec
Yield 19500 in2/lb