Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 27.4 g/m² | 17.1 lb/ream | ExxonMobil Method |
ExxonMobil Bicor™ 30MB666 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, .. |
|||
Coating Weight | 27.4 g/m² | 17.1 lb/ream | ExxonMobil Method |
ExxonMobil Bicor™ 30MBR666 OPP Film Product Description: Bicor 30MBR is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high moist.. |
|||
Coating Weight | 27.4 g/m² | 17.1 lb/ream | ExxonMobil Method |
ExxonMobil Label-Lyte® 30 LLG-101 Clear OPP Film Product Description: A clear, one-side treated, biaxially oriented polypropylene film that is used in roll-fed labeling. This film can be laminated to itself (at other gauges of LLG-101) or applied .. |
|||
Coating Weight | 27.4 g/m² | 17.1 lb/ream | ExxonMobil Method |
ExxonMobil Label-Lyte™ 30LL-101 OPP Film Product Description: A clear, one-side treated, polypropylene film that is designed to provide exceptional clarity and print protection when used as overlaminates in pressure-sensitive labeling appl.. |
|||
Coating Weight | 27.4 g/m² | 17.1 lb/ream | ExxonMobil Method |
ExxonMobil Oppalyte™ 35MD447 OPP Film Product Description: A coextruded super white opaque, modified high density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for use.. |
|||
Coating Weight | 27.4 g/m² | 17.1 lb/ream | ExxonMobil Method |
ExxonMobil Bicor® 120 CSR-2 OPP Film Product Description: Bicor CSR-2 is a one-side treated OPP film designed for cold seal release, either unsupported or as the outer web of a lamination.Availability: Latin America, North America and .. |
|||
Coating Weight | 27.4 g/m² | 17.1 lb/ream | ExxonMobil Method |
ExxonMobil Bicor® 120 SLP OPP Film Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminatin.. |