Polymer Property : Coating Weight = 19.6 lb/ream Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 31.4 g/m²
19.6 lb/ream
520
ExxonMobil Bicor® 140 BSR-ONE OPP Film
Product Description: Bicor BSR-ONE is a two-side sealable, one side treated, coextruded OPP film designed for unsupported plain or surface print applications, and in laminations on both HFFS and VF..
Coating Weight 31.4 g/m²
19.6 lb/ream
ExxonMobil Method
ExxonMobil Label-Lyte™ 35LL400 OPP Film
Product Description: A one-side treated, transparent coextruded OPP film. The film is slip controlled for optimal performance on reel-fed labeling machines.Availability: Africa & Middle East, Asia ..
Coating Weight 31.4 g/m²
19.6 lb/ream
ExxonMobil Method
ExxonMobil Oppalyte™ 40MD447 OPP Film
Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for u..