ExxonMobil Label-Lyte™ 35LL400 OPP Film

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Label-Lyte™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Label-Lyte™ 35LL400 OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A one-side treated, transparent coextruded OPP film. The film is slip controlled for optimal performance on reel-fed labeling machines.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:Outstanding optical propertiesNon-migratory slip system provides stable slip propertiesGood printabilityGood dimensional stabilityGood hot melt adhesion Applications: Beverage, AlcoholicBeverage, Carbonated Beverage, Mineral Waters Dairy ProductsHealth and Beauty Care Uses: Pressure Sensitive LabelsReel-Fed LabelsProcessing Method: Inner Web Adhesion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic PrintingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Thickness 35.6 microns
1.40 mil
ExxonMobil Method
Coating Weight 31.4 g/m²
19.6 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 205 %
205 %
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 55 %
55 %
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Modulus of Elasticity 2.00 GPa
290 ksi
MD; ExxonMobil Method
3.50 GPa
508 ksi
TD; ExxonMobil Method
Coefficient of Friction 0.30
0.30
Untreated Surface; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 5.0 %

@Temperature 135 °C,
Time 432 sec
5.0 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Shrinkage, TD 5.0 %

@Temperature 135 °C,
Time 432 sec
5.0 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
ExxonMobil Method
Gloss 85 %
85 %
45°; ExxonMobil Method
Descriptive Properties Value Comments
Yield 22100 in2/lb