Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.48 g/cc | 0.306 lb/in³ | |
Lucas-Milhaupt BRAZE 051 Silver Based Cadmium Free Filler Metal Characteristics:Braze 051 is a low cost, intermediate temperature silver brazing filler metal suitable for joining various ferrous and non-ferrous alloys that can be heated to 1650EF/900EC without d.. |
|||
Density | 8.48 g/cc | 0.306 lb/in³ | Theoretical |
Kennametal Stellite Deloro® N-6 PM with P/M Processing Adhesive wear test data: P/M 0.1, cast 0.1; Abrasive wear test data: P/M 17, cast 35. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing .. |
|||
Density | 8.48 g/cc | 0.306 lb/in³ | Theoretical |
Kennametal Stellite Deloro® N-6 PM cast Adhesive wear test data: P/M 0.1, cast 0.1; Abrasive wear test data: P/M 17, cast 35. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing .. |