Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.76 g/cc | 0.280 lb/in³ | |
Carpenter Custom 450® Stainless Steel, 25 mm Bar, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | H900 Condition |
Carpenter Custom 450® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 13-8™ H 1100 Precipitation Hardening Alloy Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 13-8™ H 950 Precipitation Hardening Alloy Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 17-4 High Strength Stainless Steel, UNS S17400 Property data below is typical of annealed samples. Available in plate. For use in fasteners, fittings, military equipment and air frame parts.Information provided by Allegheny Ludlum |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 14% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 16.4% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 2.9% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 34.5% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 43.6% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 8.5% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 409HP™ Ferritic Stainless Steel, UNS S40930 Type 409 ferritic stainless steel was introduced by Allegheny Ludlum in 1961 to provide improved oxidation and corrosion resistance for automotive exhaust systems in comparison to carbon automotive .. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | H900 Condition |
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | H900 Condition |
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
Carpenter Custom 455® Stainless Steel, Annealed, 1.27 mm Strip Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
Carpenter Custom 455® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 13-8™ H 1000 Precipitation Hardening Alloy Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 13-8™ H 1025 Precipitation Hardening Alloy Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1050°F Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1150°F Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 20% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum E-BRITE 26-1® Superferritic Stainless Steel, UNS S44627 Property data below is typical of annealed samples. High purity superferritic stainless steel. Available in sheet and strip for use in chemical process equipment to combat chloride pitting and stre.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | H900 Condition |
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Density | 7.76 g/cc | 0.280 lb/in³ | |
Carpenter Custom 455® Stainless Steel, Annealed, 25 mm Bar Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |