Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 5.85 g/cc | 0.211 lb/in³ | |
MarkeTech Ceraflex 8Y Thin Zirconia Ceramic Oxygen Ion Conductor, Yttria Stabilized Data provided by the supplier, MarkeTech International.8 mole% Y2O3 (13.8 wt%). CERAFLEX is a sintered and fully dense zirconia ceramic material that is formed into extremely thin sheets, that are .. |
|||
Density | 5.85 g/cc | 0.211 lb/in³ | |
Anderman Ceramics EZM 96 Zirconia, 96.5%, Magnesia-Stabilized Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes. |
|||
Density | 5.85 g/cc | 0.211 lb/in³ | |
Anderman Ceramics EZY 88 Zirconia, 88%, Fully Yttria-Stabilized Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes. |