Material Notes:
Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes.
Physical Properties Metric English Comments
Density 5.85 g/cc
0.211 lb/in³
Open Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Mohs 8.0
8.0
Tensile Strength 414 MPa
60000 psi
Flexural Strength 724 MPa
105000 psi
Thermal Properties Metric English Comments
CTE, linear 10.1 µm/m-°C
5.61 µin/in-°F
Thermal Conductivity 2.20 W/m-K

@Temperature 20.0 - 100 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Maximum Service Temperature, Air 1200 °C
2190 °F
Component Elements Properties Metric English Comments
MgO 3.5 %
3.5 %
ZrO2 96.5 %
96.5 %
Electrical Properties Metric English Comments
Volume Resistivity 1e+05

@Temperature 600 °C
1e+05

@Temperature 1110 °F
1.00e+13 ohm-cm

@Temperature 20.0 °C
1.00e+13 ohm-cm

@Temperature 68.0 °F
Dielectric Constant 28

@Frequency 1.00e+6 Hz
28

@Frequency 1.00e+6 Hz