Material Notes:
Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes.
Physical Properties Metric English Comments
Density 5.85 g/cc
0.211 lb/in³
Open Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Mohs 8.0
8.0
Flexural Strength 207 MPa
30000 psi
Thermal Properties Metric English Comments
CTE, linear 10.5 µm/m-°C
5.83 µin/in-°F
Thermal Conductivity 2.50 W/m-K

@Temperature 20.0 - 100 °C
17.4 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Maximum Service Temperature, Air 1800 °C
3270 °F
Component Elements Properties Metric English Comments
Y2O3 12 %
12 %
ZrO2 88 %
88 %
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm

@Temperature 600 °C
10000 ohm-cm

@Temperature 1110 °F
1.00e+13 ohm-cm

@Temperature 20.0 °C
1.00e+13 ohm-cm

@Temperature 68.0 °F
Copyright © lookpolymers.com All Rights Reserved