Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 5.70 g/cc | 0.206 lb/in³ | |
Piezo Kinetics PKI 105 Lead Metaniobate Piezoelectric Lead Metaniobate exhibits properties not usually present in other types of piezoelectric ceramics. The noteworthy facts are its low mechanical QM, negligible aging, wide range of operating temperat.. |
|||
Density | 5.70 g/cc | 0.206 lb/in³ | |
Ferro CF 7555 Low-Temperature Sealing VITREOUS Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific .. |
|||
Density | 5.70 g/cc | 0.206 lb/in³ | |
Ferro EG 4000 Display Device Glass Type: Pb-B (Composite) Typical Powder Form: VEG Typical Application: Seal Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and .. |
|||
Density | 5.70 - 6.10 g/cc | 0.206 - 0.220 lb/in³ | |
Indium Corp. NanoFoil® NF40 Nickel and Aluminum Localized Heat Source For Bonding Features:40 microns thick - optimized for bonding electronics assembliesMinimum dimension 1.2mm x 2.0mmLocalized heat source for bondingEnables high-strength, high conductivity bonds between most co.. |
|||
Density | 5.70 - 6.20 g/cc | 0.206 - 0.224 lb/in³ | |
China Tungsten ST1160 PM Antifriction Parts Information provided by China Tungsten |
|||
Density | 5.70 - 6.20 g/cc | 0.206 - 0.224 lb/in³ | |
China Tungsten ST1260 PM Antifriction Parts Information provided by China Tungsten |
|||
Density | 5.70 - 6.20 g/cc | 0.206 - 0.224 lb/in³ | |
China Tungsten ST1360 PM Antifriction Parts Information provided by China Tungsten |
|||
Density | 5.70 g/cc | 0.206 lb/in³ | |
BASF Paliotan® Yellow L 1645 Color Additive Description: Pigment combination based on Bismuth VanadatSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Amine curing system and Airdrying systemsInformation provided by.. |
|||
Density | 5.70 g/cc | 0.206 lb/in³ | |
ATI Wah Chang TI-45 Nb Applications: Aerospace Rivet Material; High Pressure Oxygenated Gas Vents; Superconducting Wire Information provided by ATI Wah Chang |