Polymer Property : Density = 0.206 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 5.70 g/cc
0.206 lb/in³
Piezo Kinetics PKI 105 Lead Metaniobate Piezoelectric
Lead Metaniobate exhibits properties not usually present in other types of piezoelectric ceramics. The noteworthy facts are its low mechanical QM, negligible aging, wide range of operating temperat..
Density 5.70 g/cc
0.206 lb/in³
Ferro CF 7555 Low-Temperature Sealing
VITREOUS Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific ..
Density 5.70 g/cc
0.206 lb/in³
Ferro EG 4000 Display Device
Glass Type: Pb-B (Composite) Typical Powder Form: VEG Typical Application: Seal Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and ..
Density 5.70 - 6.10 g/cc
0.206 - 0.220 lb/in³
Indium Corp. NanoFoil® NF40 Nickel and Aluminum Localized Heat Source For Bonding
Features:40 microns thick - optimized for bonding electronics assembliesMinimum dimension 1.2mm x 2.0mmLocalized heat source for bondingEnables high-strength, high conductivity bonds between most co..
Density 5.70 - 6.20 g/cc
0.206 - 0.224 lb/in³
China Tungsten ST1160 PM Antifriction Parts
Information provided by China Tungsten
Density 5.70 - 6.20 g/cc
0.206 - 0.224 lb/in³
China Tungsten ST1260 PM Antifriction Parts
Information provided by China Tungsten
Density 5.70 - 6.20 g/cc
0.206 - 0.224 lb/in³
China Tungsten ST1360 PM Antifriction Parts
Information provided by China Tungsten
Density 5.70 g/cc
0.206 lb/in³
BASF Paliotan® Yellow L 1645 Color Additive
Description: Pigment combination based on Bismuth VanadatSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Amine curing system and Airdrying systemsInformation provided by..
Density 5.70 g/cc
0.206 lb/in³
ATI Wah Chang TI-45 Nb
Applications: Aerospace Rivet Material; High Pressure Oxygenated Gas Vents; Superconducting Wire Information provided by ATI Wah Chang